Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 197 MPa | 28500 psi | ASTM D882 |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |