1% Secant Modulus, MD 290 MPa
42000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
1% Secant Modulus, MD 290 MPa
42000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
1% Secant Modulus, MD 290 MPa
42000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308FK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processabilityIncreased stiffnessGood toughnessUse alone or in blends with LDPE o..
1% Secant Modulus, MD 290 MPa
42000 psi
ASTM D882
ExxonMobil Exceed™ 1327CA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327CA is a metallocene ethylene-hexene copolymers. It produces films which have high modulus whilst retaining good toughness. These properties together with excellent dr..
1% Secant Modulus, MD 290 MPa
42000 psi
ASTM D882
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula..