Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 310 MPa | 45000 psi | ASTM D882 |
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
1% Secant Modulus, MD | 310 MPa | 45000 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 310 MPa | 45000 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |