Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 331 MPa | 48000 psi | ASTM D882 |
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009.. |
|||
1% Secant Modulus, MD | 331 MPa | 48000 psi | ASTM D882 |
LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade PETROTHENE NA272130 is a medium density polyethylene resin designed for overwrap film applications. NA272130 exhibits good film optics and high stiffness.Regulatory Status: NA272130 meets the requir.. |