Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 27.8 MPa | 4030 psi | ASTM D882 |
ExxonMobil ESCOR™ AT 320 Blown Film Resin
(discontinued **) ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical |