Polymer Property : 1% Secant Modulus, MD = 49300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 340 MPa
49300 psi
ASTM D 882
NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin
TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur..