Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 65.0 MPa | 9430 psi | ISO 527-3 |
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,.. |
|||
1% Secant Modulus, MD | 65.0 MPa | 9430 psi | ISO 527-3 |
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep.. |
|||
1% Secant Modulus, MD | 65.0 MPa | 9430 psi | ISO 527-3 |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |