Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 689 MPa | 100000 psi | ASTM D822 |
LyondellBasell Alathon® M6030 High Density Polyethylene ApplicationsALATHON M 6030 is a medium molecular weight high density homopolymer with extremely low gel content. Typical applications for this resin are cast film, coextrusion and dry food packagin.. |