Mechanical Properties Metric English Comments
1% Secant Modulus, MD 630 MPa
91400 psi
ASTM D 882
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin
17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..