Polymer Property : 1% Secant Modulus, TD = 100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 100 MPa
14500 psi
ISO 527-3
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene
Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h..
1% Secant Modulus, TD 100 MPa
14500 psi
ISO 527-3
Polimeri Europa Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene
Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexi..
1% Secant Modulus, TD 100 MPa
14500 psi
ISO 527-3
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene
Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even..