Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 790 MPa | 115000 psi | ASTM-D882 |
Braskem HD3000N HDPE Cast Film Extrusion Polyethylene Homopolymer HD3000N is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for cast film extrusion. It offers high processability, stiffness, and good impact resist.. |