Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 830 MPa | 120000 psi | ISO 527-3 |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
1% Secant Modulus, TD | 827 MPa | 120000 psi | ASTM D822 |
LyondellBasell Alathon® M6030 High Density Polyethylene ApplicationsALATHON M 6030 is a medium molecular weight high density homopolymer with extremely low gel content. Typical applications for this resin are cast film, coextrusion and dry food packagin.. |