Polymer Property : 1% Secant Modulus, TD = 1270 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1270 MPa
184200 psi
ASTM D882
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin
Features: Excellent barrier propertiesHigh stiffnessGood processability Low gel Applications: Barrier filmsCo-extrusionDry food packagingInformation provided by Nova Chemicals