1% Secant Modulus, TD 91.0 MPa
13200 psi
ASTM D882
LyondellBasell Ultrathene® UE637000 Ethylene Vinyl Acetate Copolymer, Film Extrusion Grade
ULTRATHENE UE637000 is an EVA copolymer with good toughness, flexibility and clarity. Applications include laminating and heavy duty films as well as injection and blow molding. UE637000 contains no..
1% Secant Modulus, TD 91.0 MPa
13200 psi
ASTM D882
LyondellBasell Ultrathene® UE672006 Ethylene Vinyl Acetate Copolymer, Film Grade
Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w..
1% Secant Modulus, TD 91.0 MPa
13200 psi
ASTM D882
LyondellBasell Ultrathene® UE672102 Ethylene Vinyl Acetate Copolymer, Film Grade
Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w..
1% Secant Modulus, TD 91.0 MPa
13200 psi
ASTM D882
LyondellBasell Ultrathene® UE672317 Ethylene Vinyl Acetate Copolymer, Film Grade
Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w..