1% Secant Modulus, TD 144 MPa
20900 psi
ASTM D 882
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin
FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0..
1% Secant Modulus, TD 144 MPa
20900 psi
ASTM D882
ExxonMobil LD 307.76 Clear, High Impact Film Resin
LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical