Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 152 MPa | 22000 psi | ASTM D882 |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
1% Secant Modulus, TD | 152 MPa | 22000 psi | ASTM D882 |
Westlake EF677 Low Density Polyethylene Westlake EF677 is a high melt index LDPE resin suggested for garment films, or other applications requiring excellent drawdown. This material is also an excellent choice for PE foam applications.App.. |
|||
1% Secant Modulus, TD | 152 MPa | 22000 psi | ASTM D882 |
Westlake Elevate™ EF437 2.5% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
1% Secant Modulus, TD | 152 MPa | 22000 psi | ASTM D882 |
Westlake LF2040 Hexene Linear Low Density Polyethylene Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
1% Secant Modulus, TD | 152 MPa | 22000 psi | ASTM D882 |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |