Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1590 MPa
230000 psi
ASTM D882
ExxonMobil HDPE HD 7845.30 High Density Polyethylene Resin
Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc..
1% Secant Modulus, TD 1590 MPa
230000 psi
ASTM D882
ExxonMobil HD 7845.30 MMW Blown Film Resin
Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc..