Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 120 MPa | 17400 psi | ASTM D882 |
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin Features: Exceptional puncture resistanceVery good tear propertiesLow gel levelExcellent optical properties Excellent elongation characteristics Easy to process, no drying required Applications: Cas.. |