Polymer Property : 1% Secant Modulus, TD = 176 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 176 MPa
25500 psi
ASTM D882
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin
Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals
1% Secant Modulus, TD 176 MPa
25500 psi
ASTM D882
ExxonMobil Exceed™ 2018EB Blown Film Resin  (discontinued **)
Exceed 2018EB resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals Exxpol® Technology. The higher melt index makes this polymer ideally sui..