Polymer Property : 1% Secant Modulus, TD = 17900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 123 MPa
17900 psi
ASTM D882
ExxonMobil LL 3002.32 Cast Film Resin  (discontinued **)
LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, ..