Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, TD = 218000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1500 MPa
218000 psi
ASTM D882
SABIC F00952 High Density Polyethylene for Blown Film
Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
1% Secant Modulus, TD 1500 MPa
218000 psi
ASTM D882
SABIC F00952EQ High Density Polyethylene for Blown Film
Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect..
1% Secant Modulus, TD 1500 MPa
218000 psi
ASTM D882
SABIC FJ00952 High Density Polyethylene for Blown Film
Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, ..
Copyright © lookpolymers.com All Rights Reserved