Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 196.14 MPa | 28447 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin
(discontinued **) LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne.. |
|||
1% Secant Modulus, TD | 196.14 MPa | 28447 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin
(discontinued **) LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud.. |
|||
1% Secant Modulus, TD | 196.14 MPa | 28447 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin
(discontinued **) LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down.. |
|||
1% Secant Modulus, TD | 196.14 MPa | 28447 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF2021 Linear low density polyethylene resin
(discontinued **) LF2021 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown and cast film extrusion which offers outstandin.. |
|||
1% Secant Modulus, TD | 196.14 MPa | 28447 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin
(discontinued **) LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
1% Secant Modulus, TD | 196.14 MPa | 28447 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin
(discontinued **) LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
1% Secant Modulus, TD | 196.14 MPa | 28447 psi | ASTM D882 |
Lotte Chemical Titan TITANLENE® LDF264YZ Low density polyethylene LDF264YZ is a low density polyethylene resin for film extrusion. LDF264YZ has no slip and anti-block additives. LDF264YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |