Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 221 MPa @Thickness 0.0250 mm |
32100 psi @Thickness 0.000984 in |
ASTM D882 |
Equate EFDA-7047 LLDPE Film Extrusion Resin EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does n.. |
|||
1% Secant Modulus, TD | 221 MPa @Thickness 0.0250 mm |
32100 psi @Thickness 0.000984 in |
ASTM D882 |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |