Polymer Property : 1% Secant Modulus, TD = 37700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 260 MPa
37700 psi
ASTM D882
SABIC 218 Series Linear Low Density Polyethylene for Blown Film
Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a..
1% Secant Modulus, TD 260 MPa
37700 psi
3 mil; ASTM D882
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin
Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial ..