Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 262 MPa | 38000 psi | ASTM D882 |
ExxonMobil Exceed™ 1023CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1023CA is a metallocene ethylene-hexene copolymers. The slightly higher stiffness of Exceed 1023CA makes it easier to process on certain filling machinery, whilst still k.. |
|||
1% Secant Modulus, TD | 262 MPa | 38000 psi | ASTM D882 |
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
1% Secant Modulus, TD | 262 MPa | 38000 psi | ASTM D882 |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
1% Secant Modulus, TD | 262 MPa | 38000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
1% Secant Modulus, TD | 262 MPa | 38000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |