1% Secant Modulus, TD 270 MPa
39200 psi
ASTM D882
SABIC 118 Series Linear Low Density Polyethylene for Blown Film
Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st..
1% Secant Modulus, TD 270 MPa
39200 psi
ASTM D882
SABIC 120W Linear Low Density Polyethylene for Blown Film
Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti..
1% Secant Modulus, TD 270 MPa
39200 psi
ASTM D882
SABIC 518N Linear Low Density Polyethylene for Blown Film
Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug..
1% Secant Modulus, TD 270 MPa
39200 psi
ASTM-D882
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer
LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid ..