Mechanical Properties Metric English Comments
1% Secant Modulus, TD 423 MPa
61400 psi
ASTM D882
ExxonMobil LL 3402.48 Cast Film Resin  (discontinued **)
LL 3402.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex..