Polymer Property : 1% Secant Modulus, TD = 46400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 320 MPa
46400 psi
ASTM D882
SABIC 726 Series Linear Low Density Polyethylene for Blown Film
Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher ..