Mechanical Properties Metric English Comments
1% Secant Modulus, TD 365 MPa
53000 psi
ASTM D882
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..