Mechanical Properties Metric English Comments
1% Secant Modulus, TD 586 MPa
85000 psi
ASTM D882, A
Total MDPE HL 323 Medium Density Polyethylene, Film Resin
Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st..