Mechanical Properties Metric English Comments
1% Secant Modulus, TD 59.1 MPa
8570 psi
ASTM D882
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s..