Polymer Property : 1% Secant Modulus, TD = 64000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 441 MPa
64000 psi
ASTM D882
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..
1% Secant Modulus, TD 441 MPa
64000 psi
ASTM D882
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..
1% Secant Modulus, TD 441 MPa
64000 psi
ASTM D882
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..