1% Secant Modulus, TD 79.3 MPa
11500 psi
D882
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength m..