Mechanical Properties Metric English Comments
1% Secant Modulus, TD 883 MPa
128000 psi
1 in/min; ASTM D882
Total HDPE 6420 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with..