Polymer Property : 1% Secant Modulus, TD = 96.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 96.5 MPa
14000 psi
ASTM D882
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b..