Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 2750 g/25 mm | 2750 g/in | F-88-68(73) |
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar®EZS is a high slip version of EZ. Used where a premium product appearance i.. |