Mechanical Properties Metric English Comments
Seal Strength 300 g/25 mm

@Pressure 0.138 MPa,
Temperature 115 °C
300 g/in

@Pressure 20.0 psi,
Temperature 239 °F
0.8 sec, Untreated; ExxonMobl Method
ExxonMobil Bicor™ 15MB400 OPP Film
Product Description: Bicor 15MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou..
Seal Strength 300 g/25 mm

@Pressure 0.138 MPa,
Temperature 115 °C
300 g/in

@Pressure 20.0 psi,
Temperature 239 °F
EMS, 0.8 sec, Untreated; ExxonMobl Method
ExxonMobil Bicor™ 20MB400 OPP Film
Product Description: Bicor 20MB400 is a one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:..
Seal Strength 300 g/25 mm

@Pressure 0.138 MPa
300 g/in

@Pressure 20.0 psi
0.8 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 38DO447 OPP Film
Product Description: A super white opaque BOPP film. The Diamex technology allows for super low density and very high yield. Diamex makes it possible to lower the density, without decreasing the mod..
Seal Strength 300 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
300 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 38ICE OPP Film
Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal ..
Seal Strength 300 g/25 mm

@Pressure 0.138 MPa,
Temperature 115 °C
300 g/in

@Pressure 20.0 psi,
Temperature 239 °F
0.8 sec, Untreated; ExxonMobl Method
ExxonMobil Bicor™ 17MB400 OPP Film
Product Description: Bicor 17MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou..
Seal Strength 300 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
300 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 33ICE OPP Film
Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on..