Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 18MB090 OPP Film Product Description: Biaxially oriented polypropylene film metallizable on one side, with a slip controlled broad seal range surface on the other side. Once metalized, film designed to be used in la.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 20MB080 OPP Film Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 29MB080 OPP Film Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Metallyte™ 15MM348 OPP Film Product Description: An enhanced barrier metalized film with a very broad seal range and can be considered a multipurpose film. This designed of this film allow excellent performance on HFFS machine.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM348 OPP Film Product Description: An enhanced barrier metalized film with a very broad seal range designed to be used in laminate with OPP or Polyester for HFFS applications. The design of this film allows excel.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM383 OPP Film Product Description: A biaxially oriented very high barrier metalized polypropylene film. This film offers an outstanding moisture barrier and a broad seal range surface on the other side. This film.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM388 OPP Film Product Description: A metallized biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance p.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM483 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance packaging ap.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
460 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM488 OPP Film Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c.. |
|||
Seal Strength | 460 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
460 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW647 OPP Film Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & .. |