Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 9.40 g/25 mm | 9.40 g/in | Release Adhesion, 180° Peel; ASTM D1000 |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Seal Strength | 9.40 g/25 mm | 9.40 g/in | Release Adhesion, 180° Peel; ASTM D1000 |
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 9.40 g/25 mm | 9.40 g/in | Release Adhesion, 180° Peel; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 9.40 g/25 mm | 9.40 g/in | Release Adhesion, 180° Peel; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 9.40 g/25 mm | 9.40 g/in | Release Adhesion, 180° Peel; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 9.40 g/25 mm | 9.40 g/in | Release Adhesion, 180° Peel; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-12020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 9.40 g/25 mm | 9.40 g/in | Average value: 9.40 g/25 mm Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |