Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.614 kN/m | 3.50 pli | 180° peel, PET/s.s. |
Dielectric Polymers NT-101PLE Double Liner Tape
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft base release and high density PE interliner.Features: Polyethylene interliner permits selective diecuttingPlasticizer migration resistantChemica.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7026 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7052 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7045 and 7052 are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™.. |
|||
Peel Strength | >= 0.614 kN/m | >= 3.50 pli | Bond Strength |
Arlon 44571B008 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7025 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polypropylene, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7028FL Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7029 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polypropylene, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7031 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7033 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7052W Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™ Adhesive P140.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Adhesion to Acrylic enamel |
3M Controltac™ 8620Cv3 ES Changeable Graphic Film with Comply™ v3 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |