Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7026 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7811 Dot Matrix Printable Polyimide Label Material 3M™ Dot Matrix Printable Polyimide Label Material 7811 is a polyimide film product that offers ultra-high temperature performance. This label product utilizes 3M™ Adhesive 100, that can withstand .. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM040 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM042 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM045 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7025 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7031 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7033 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7045 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7045 and 7052 are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7052W Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™ Adhesive P140.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7911FL Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | 12 in/min, 90° pullback, Aluminum Rail |
3M Diamond Grade™ 983 Conspicuity Markings 3M™ Diamond Grade™ Conspicuity Markings Series 983 are highly retrorflective micro-prismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detection. The ref.. |
|||
Peel Strength | 0.614 kN/m | 3.50 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM048 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |