Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.0400 - 7.20 kN/m
0.228 - 41.1 pli
Average value: 1.93 kN/m Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Peel Strength 0.0400 kN/m
0.228 pli
Adhesion to PET; TP-141
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.Uses: S..
Peel Strength 0.0400 kN/m
0.228 pli
Aluminum Foil; ASTM D-1876-72
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.Uses: S..