Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.0438 kN/m | 0.250 pli | Adhesion to Steel; ASTM D3330 |
3M 25A12 Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tape has a low-tack adhesive system to help provide temporary protection of many polished steel and aluminum sheets, coils, gloss finish plastic laminate top.. |
|||
Peel Strength | 0.0438 kN/m | 0.250 pli | Adhesion to Steel; ASTM D3330 |
3M 3051 Low Tack Paper Tape 3M™ Low Tack Paper 3051 is designed to apply easily and remove cleanly from a variety of surfaces.Information provided by 3M |
|||
Peel Strength | 0.0438 kN/m | 0.250 pli | Adhesion to Steel; ASTM D3330 |
3M 2112 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2112 has a very low-tack adhesive system to help provide temporary protection of many polished metals, smooth plastics and glass materials with minimum adhesion bu.. |
|||
Peel Strength | 0.0438 kN/m | 0.250 pli | Adhesion to Steel; ASTM D3330 |
3M 2A12 (Clear) Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tapes have a low-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M |
|||
Peel Strength | 0.0438 kN/m | 0.250 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.0438 kN/m | 0.250 pli | Adhesion to Steel; ASTM D3330 |
3M 51825 Industrial Polyethylene Temporary Surface Protection Tape 3M™ Industrial Polyethylene Temporary Surface Protection Tape51825 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided by.. |
|||
Peel Strength | 0.0438 kN/m | 0.250 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.0438 kN/m | 0.250 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |