Polymer Property : Peel Strength = 0.220 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.220 kN/m
1.26 pli
Adhesion to PET; TP-141
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane
Features: Hard, flexible, abrasion resistant coatings. Primarily used for all solution binder for inks and lacquers on fabrics and various substrates.Uses: Adhesives and inks & lacquers, pigment bin..