Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.38347 kN/m | 2.1875 pli | Adhesion to steel; ASTM D1000 |
3M 1345 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Adhesion to Steel; ASTM D3330 |
3M 33315 Copper Foil Tape "Tinned," corrosion resistant.Information provided by 3M |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Adhesion to Steel; ASTM D3330 |
3M 3369 General Purpose Aluminum Foil Tape Thinnest aluminum foil tape. UL 723 Classified.Information provided by 3M |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1060H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1115 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1220 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1915S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | ABS, 180° Peel, 10 min dwell; ASTM D3330 |
3M 8417 Polyester Film Tape 3M™ Polyester Film Tape 8417 is a self-wound (linerless) transparent polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. It is often used as an overlaminate in conjunction with 3.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | 90° Peel, PET/PET, Initial (20 mins); ASTM D3330 |
3M 9061MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | H.D. Polyethylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485EK Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1115 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1115 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1120 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.38347 kN/m | 2.1875 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1915M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |