Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.00 kN/m | 5.71 pli | Bell Peel |
Henkel Hysol EA 9321 Paste Adhesive System Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair |