Polymer Property : Peel Strength = 1.47 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.47 kN/m
8.40 pli
(S1 to S1) Bond Strength; Arlon-SQA-TMS-011
Arlon 51112R013 0.013" (0.330 mm) Cured, Self Fusing, Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured, Self Fusing, Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data sho..
Peel Strength 1.47 kN/m
8.40 pli
To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
Arlon EP2 Enhanced Polyimide Laminate and Prepreg
High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications ..
Peel Strength 1.47 kN/m
8.40 pli
(S1 to S1), Bond Strength; Arlon SQA-TMS-011
Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Peel Strength 1.47 kN/m
8.40 pli
Bond Strength; ASTM D624
Arlon 55359R062 62 mil Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materi..
Peel Strength 1.47 kN/m
8.40 pli
180°, Aluminum, 50% RH
3M PN8017 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Peel Strength 1.47 kN/m
8.40 pli
180°, Aluminum, 50% RH
3M PN8019 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Peel Strength 1.47 kN/m
8.40 pli
180°, Aluminum, 50% RH
3M PN8027 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Peel Strength 1.47 kN/m
8.40 pli
180°, Aluminum, 50% RH
3M PN8029 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..