Polymer Property : Peel Strength = 1.75 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.877 - 1.75 kN/m
5.00 - 10.0 pli
T-peel, Al to Al
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy
Description: Master Bond Supreme 10AOHT-LO has a combination of properties consisting of excellent thermal conductivity, superior electrical insulation, great adhesion to a wide variety of substrate..
Peel Strength 0.877 - 1.75 kN/m
5.00 - 10.0 pli
T-peel, Al to Al
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System
Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat..
Peel Strength 0.877 - 1.75 kN/m

@Temperature -55.0 °C
5.00 - 10.0 pli

@Temperature -67.0 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 0.877 - 1.75 kN/m

@Temperature -55.0 °C
5.00 - 10.0 pli

@Temperature -67.0 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..