Mechanical Properties Metric English Comments
Peel Strength 1.82 kN/m
10.4 pli
Bond Strength (S2 to S2); Arlon SQA-TMS-011
Arlon 18146R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi..