Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.895 kN/m | 10.81 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 4.9 mil; ASTM D3330 |
3M 9502 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 1.895 kN/m | 10.81 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 4.9 mil; ASTM D3330 |
3M 9505 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 1.895 kN/m | 10.81 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 4.9 mil; ASTM D3330 |
3M 9552 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 1.895 kN/m | 10.81 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 4.9 mil; ASTM D3330 |
3M 9555 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |